/images/store/162/Concrete_Pour_pict.jpg/images/store/162/Concrete_Pour_Trowel_3.jpg/images/store/162/Contractor_W-Plans_6.jpg
/images/store/162/CraneSunset.jpg/images/store/162/Drywall_App_4.jpg/images/store/162/Grading_5.jpg
/images/store/162/Industrial_pict.jpg/images/store/162/Masonry_App_7.jpg/images/store/162/Masonry_pict.jpg
/images/store/162/Plywood_pict.jpg/images/store/162/Tilt-Up_Workers_App_2.jpg/images/store/162/Tilt-Up_Workers_App_4.jpg
 

Search:

Sponge Rubber EXP Expansion Joint

Sponge Rubber EXP Expansion Joint

Right Pointe

Sponge Rubber Expansion Joint is composed of economical re-bonded sponge rubber particles manufactured to a consistent density and size. This very workable material has a recovery rate of 95% or more of the original thickness and a density exceeding 30 pounds/cu. ft.

(click image to enlarge)
Quick Overview
    Features and Benefits:
  • Designed for high performance, low tolerance criteria projects
  • Excellent recovery properties for installations with wide temperature variations
  • For isolation applications or between materials with dissimilar coefficients of expansion
  • Meets or exceeds all specifications.
  • Resilient - recovers 95% of original thickness after compression.
  • Resists water infiltration.
  • Easy to handle and install
  • Petroleum resistant


  • Use And Applications:
    Sponge Rubber Expansion Joint is suitable for use with a wide variety of concrete construction projects. Noted for its excellent recovery properties, it is frequently used in applications that experience rapid changes in temperature.

    Click here for the MSDS
Interested in this item or want more information?

Phone:
Email:

Can't find what you want? Give us a call and we can help you find it.
Details
Size Information: Thickness: 1/4", 3/8", 1/2", 3/4", 1"
Standard Lengths: 54"
Slab Width: 36"
Cut to Size: 2" to 36" in 1/2" increments

Typical Properties:
  • Compression (to 50% of original) 50-500psi
  • Water Absorption by Weight Average of closed and open-celled sponge Compression Set 10% maximum. ASTM Method: ½" samples compressed for 22 hours @ 70°F - 24 hour recovery
  • Density 30 PCF minimum
  • Temperature Resistance Low -40°F
  • Temperature Resistance High Continuous +180°F
  • Temperature Resistance High Intermittent +220°F
  • Accelerated Aging: Good
  • ASTM Method: 7 days at 158°F-lineal shrinkage maximum 2%) Flexibility 180° bend without cracking
  • Tensile Strength (minimum) 25psi
  • Elongation (minimum) 75%
  • Additional Information